the16bitgamer@programming.dev to 3DPrinting@lemmy.worldEnglish · 26 days agoPerfectly dry filament, as all filament should beprogramming.devimagemessage-square15fedilinkarrow-up1192arrow-down12file-text
arrow-up1190arrow-down1imagePerfectly dry filament, as all filament should beprogramming.devthe16bitgamer@programming.dev to 3DPrinting@lemmy.worldEnglish · 26 days agomessage-square15fedilinkfile-text
This took forever to get right, but all my filament dryboxes are at 10% and I can’t get it any lower.
minus-squarejokeyrhyme@lemmy.mllinkfedilinkEnglisharrow-up3·25 days agofor some filament, at least PLA and PETG, you don’t want to filament entering the extruder to be too warm because it can soften and cause jams / under-extrusion
for some filament, at least PLA and PETG, you don’t want to filament entering the extruder to be too warm because it can soften and cause jams / under-extrusion