Full brims, mouse ears, with glue, without glue, higher bed temperature, lower bed temperature, flat base, concentric cutout base - whatever I try, I seem to be getting wank adhesion, major warping, and ultimately this shitshow.

Dry PLA, warm room, no draught, plate cleaned with IPA. I’m going to fucking punch this thing in its stupid fucking face.

Edit: Prevailing advice very much seems to be to bust out the Fairy liquid and give it a good scrub, so I’ll try that. It’s a Kobra Neo 2 so is auto-levelling, so I can’t piss around with any of that stuff (as far as I know). Another quick question while I think about it, does everyone always print onto the bed at ~60°C? Because Orca Slicer’s default for a textured PEI plate is 45°C, which seems mad. I think I tried it once and it was shite so turned it back up to 60.

  • KairuByte@lemmy.dbzer0.com
    link
    fedilink
    English
    arrow-up
    3
    ·
    2 days ago

    I need to point out, IPA isn’t magical. If you’re just giving it a quick swipe, or mopping it around, you’re not actually cleaning it you’re just moving the mess around. It’s fine for some in between stuff, but scrubbing with soap and warm water is going to be much more efficient at cleaning the plate.

    • vodka@feddit.org
      link
      fedilink
      English
      arrow-up
      3
      ·
      2 days ago

      This is so important, you gotta wash the print surface, not disinfect it.

      Wiping it with alcohol is good and all, but it needs some dishwashing detergent and a soft sponge every now and then.